HERCULES
SEALCOAT MANUFACTURING, inc
RECENT
D.O.T. TEST DATA.
|
STAR MACRO-DECK |
|
|
|
|
|
|
|
SOLIDS |
PERMEABILITY, DAYS |
% DECREASE |
|
|
|
|
% WT. |
28 |
56 |
IN PERMEABILITY. |
|
|
STAR
MACRO-DECK |
20 |
2878 |
1816 |
25.86% |
49.68% |
|
STAR
MACRO-DECK/WATER (1/1) |
10 |
3074 |
2390 |
20.81% |
33.78% |
|
STAR
MACRO-DECK (1/2) |
7 |
3403 |
3280 |
12.34% |
9.12% |
|
CONTROL-NO
MACRO-DECK |
0 |
3882 |
3609 |
0.00% |
0.00% |
|
|
|
|
|
|
|
|
Standards of Permeability Tests |
|
|
|
|
|
|
Permeability (Sample) |
|
Number
Range |
General
Situation Applied |
|
|
|
High |
|
>4000 |
High w/c ratio )=0.60 |
|
|
|
Moderate |
|
2000-4000 |
Moderate w/c
ratio )=0.4-0.5 |
|
|
|
Low |
|
1000-2000 |
Low w/c ratio (Iowa dense Concrete) |
||
|
Very
Low |
|
100-1000 |
Latex Modified concrete |
|
|
|
Negligible |
|
<100 |
Polymer integrated polymer concrete. |
||